Shandong, China
Business Type:
Manufacturer/Factory, Trading Company
Type of Ownership:
Limited Company
Management System Certification:
ISO 9001
Export Year:
Terms of Payment:
LC, T/T, D/P, Western Union, Small-amount payment, Money Gram
OEM/ODM Service
Sample Available
U.S. Warehouse

Welding Flux, Welding Material, Agglomerated Flux manufacturer / supplier in China, offering Welding Wire Combined with Welding Flux, Synthetic Staple Fibers Needle Punched Geotextile, Round Ductile Iron Manhole Cover with Frame and so on.

Gold Member Since 2006
Audited Supplier
Supplier Homepage Products welding flux Welding Wire Combined with Welding Flux

Welding Wire Combined with Welding Flux

Get Latest Price
Min. Order / Reference FOB Price
1 Ton US $350-500/ Ton
Port: Qingdao, China
Production Capacity: 15000tons Per Year
Payment Terms: L/C, T/T, D/P, Western Union, Money Gram
state: Solid
pH: Alkaline
Type: Inorganic
Melting Point: >600℃
Chemical Composition: SiO₂=10%-30%
Function: Protect Weld Metal

You Might Also Like


Basic Info

Model NO.: welding flux
Application: Submerged-arc Welding
Manufacturing Method: Agglomerted
Kind: Fluorine Alkali
Grain Size: 10-60 Meshes
Performance: Easy to Deslag
Color: Grey
Usage: Weld Structure Steel, Pressure Vessel etc
Suitable: Low Carbon Low Alloy Steel
Delivey: 15-20 Days
Payment: Tt or LC
Packages: Paper Bag or Pallet
Port: Qingdao
Trademark: trustworthy
Transport Package: Kraft Paper Bag or Woven Bag
Specification: sj101
Origin: Shandong China

Product Description

Submerged arc welding flux

1. the welding flux is fluorine alkali type sintered flux. 
2. Grain size: 10-60(2.0-0.3mm) meshes. 
3. Performance: 
A. Easy to deslag. 
B. Sulfur removal, phosphor removal and anti-rust. 
C. Fine appearance of weld (even in the narrow gap of deep slope entrance). 
D. Metal welding seam: Good plastic toughness, low hydrogen content diffusion and fine properties of cold, heat and crack resistance. 

1. the welding flux is For low carbon, low alloy and pipeline steel. 
2. For thick wall structures of different high-tensile steels. 

1. The oil contamination, moisture, iron rust and other foreign substances must beremoved from the welding joint. 
2. It is better to weld under direct current. 
3. Welding flux must be baked under 250-300°C for more than 2 hours
Before usage. 

Chemical Compositions: (%)
25~3025~3015~2015~20≤ 0.05

Basicity of the flux: B/w=1.6--1.8
Mechanial performance of the deposited metal: 

WiresStandard ModelsS

Welding Wire Combined with Welding FluxWelding Wire Combined with Welding FluxWelding Wire Combined with Welding Flux